Requirements for Raw Materials Used in Cold Heading

May 14, 2026 Leave a message

1. High plasticity and low hardness are required.
Since tangential tensile stress acts on the lateral surface of the blank during cold heading-making it prone to longitudinal surface cracking-materials specifically characterized by high plasticity and low hardness must be used. For steel materials, the surface hardness is generally required to be in the range of 75–85 HRB.

 

2. High surface quality is required.
As the cold heading process is primarily used to manufacture standard parts (such as screws and bolts) that typically undergo no subsequent machining, the shank sections-which experience minimal deformation during the process-retain the blank's original surface. Consequently, the raw materials must possess low surface roughness and be free from surface defects such as scratches, pitting, or rust.

 

3. High dimensional accuracy is required.
To ensure the accuracy of the blank's volume, strict tolerances on the blank's diameter are required. Taking an M10×1.5 bolt as an example, the nominal size and tolerance of the raw material are Φ...

Send Inquiry

Send Inquiry